Injection Mold Design Tips
Mold Layout, Inserts, and Assembly

The slide guide rails should be at least one-third as high as the slide to keep it stable and ensure smooth travel.
Machine lubrication grooves wherever surfaces slide against each other. Use closed-end grooves to keep lubricant from flowing out. A single milling cutter can usually cut the grooves directly on a milling machine.
For small molds, wire EDM is generally used to machine the pockets that seat the core and cavity blocks. This improves mold accuracy. For larger molds, these pockets are usually milled. Check the perpendicularity of the pocket walls. Mill a 0.2-deep relief around the pocket perimeter so the block can seat fully during assembly.
Provide a 1° assembly taper where an insert fits into a core or cavity block, where two blocks interlock, or where a block fits into the mold base. This prevents damage during assembly.
At the insert seating feature, use a length tolerance of −0.02 and a size tolerance of −0.10. Use +0.02 for the corresponding seating feature in the core or cavity block.
For a chamfered insert, use a tolerance of +0.01 on the distance from the bottom of the insert to the chamfer to prevent flash.
Use NAK80 for the main blocks of the housing mold. Use SKH9 or SKH51 for inserts and pins, with optional nitriding [1]. VIKING may be used where needed.
After drawing the part, determine the slide locations and sizes first. Check for interference and adequate strength before sizing the core and cavity blocks.
Set the insert size tolerance to −0.01 and the corresponding insert pocket tolerance to +0.01.
Use R0.20 at the internal corners of a square opening cut by wire EDM. Use R0.20 on the matching insert corners. This accounts for the wire diameter and helps prevent corner wear and flash.
The recess for a ball detent is typically conical, with a base diameter of Ø3 and an included angle of 90°–120°.
Give the fixed half more draft than the moving half so the part stays on the moving half when the mold opens. This also helps prevent deformation. Uneven pull from the fixed half can warp long, thin-walled parts or cause them to stick to that half.
Use a two-stage side core pull when the side core requires a high extraction force and the part has tight tolerances.
The slide locking wedge angle equals the angle pin angle plus 2°. Typical locking wedge angles are 18°, 20°, or 22°.
Follow these practices during mold assembly:
- Blow off the core and cavity blocks, cavity surfaces, inserts, runner plate, and parting surfaces with an air gun.
- Stone the surfaces of the core and cavity blocks, cavity surfaces, inserts, and parting surfaces before assembly so the components fit smoothly.
- Clear the corners to prevent interference and damage.
- Plan how the subsequent work will be carried out before assembling the mold.
On large molds, design the side clamps for the core and cavity blocks so their tops sit 0.5–1.0 mm below the parting surface when tightened. This prevents interference.
The mold shrinkage for PC+GF20 is 3/1000.
The typical mold shrinkage for POM is 20/1000, but some areas can reach 30/1000.
Gate Breakaway, Ejection, and Parting Surfaces
To keep a tunnel gate from scratching the part during ejection, add a wedge-shaped feature in the runner 2–4 mm from the gate. Make it about half the runner height with a 10° angle per side. It helps break the gate during ejection.
Make the sprue puller well an inverted cone, 8–10 mm deep, with a 10° taper per side and a top diameter equal to the runner width. This keeps the puller feature from snagging the runner during ejection, which can otherwise occur with a puller ground to a wedge on one side.
There are two types of parting locks:
- A rubber parting lock. A central screw adjusts the deformation of the rubber and therefore the holding force.
- A spring-steel parting lock. Both types delay separation of the fixed and moving halves in three-plate pinpoint-gate molds.
Some molds use an early ejector return mechanism or a microswitch to ensure that the ejector pins and lifters have returned. Mount the female half of the early return mechanism on plate 108 and the male half on plate 102. The male component resembles an ejector pin and is retained at its base by a headless screw. Two mechanisms are typically fitted. The microswitch is installed between plates 108 and 109, with the electrical components mounted on plate 109.
Check the thickness of the fixed-side and moving-side clamping plates against the bolt length available for mounting the mold in the injection molding machine. Mill the four corners lower if needed. For added security, four bolting holes can be drilled in the plates to match the hole pattern on the machine platens.
The forming end of a lifter has a straight land, typically 4–6 mm long. Add a 0.5–1 mm radius at the bottom to ensure smooth lifter travel between plates 107 and 108 during ejection.
On cosmetic parts that require texture, select the draft angle for the texture depth to prevent drag marks. Machine some projecting features 0.02–0.03 undersize per side to allow for the increase in cross section after texturing.
To control the mismatch step at mold closure, make the fixed half 0.03–0.05 smaller per side than the moving half.
On some slide molds, machine a lubrication groove into the angled contact face between the slide and its locking wedge. When molding is unaffected, a groove on the top of the mold plate is quicker to machine than one on the underside of the slide.
Keep the parting line away from areas with specified surface requirements.
In fiber-filled materials, mold shrinkage is 1–2 parts per thousand lower in the flow direction than across the flow. Unfilled materials show the reverse relationship.
Shrinkage at the gear tip circle is 1–2 parts per thousand lower than at the root circle.
Core and cavity blocks may need rework after the mold has been in service. Minimize the use of oilstones, since repeated stoning can alter the mold profile. Use shaped softwood or a soft bamboo stick instead.
On molds with slides, add four support pillars between plates #102 and #103.
Consider a two-stage core pull when a part is molded around an internal insert and enclosed by the surrounding cavity block. This can prevent difficult demolding and part damage. If the insert is on the fixed side or on a slide, it is often withdrawn first. If it is on the moving side and shuts off against the fixed side, deepen the counterbore for the insert so the part is ejected first and the insert is withdrawn afterward. If there is no shutoff, withdraw the insert first and change the mold design accordingly.
If a flat shutoff between the fixed and moving halves is not perpendicular to the mold-opening direction, design it as an angled shutoff. This reduces wear-related flash and creates preload when the mold closes, improving contact. Allow a positive length tolerance of +0.02. If the two halves have opposing draft directions, check the angled shutoff carefully. It can leave a witness line that differs from the original part drawing, hard-to-remove flash, or a mismatch step.
If the fixed half is to be textured, make its profile 0.03–0.05 mm smaller per side, as appropriate for the texture depth.
Surface Finish, Gate Design, and Machining

For fine polishing of electrodes, typically use 1000-grit abrasive paper. Use 1200 grit or finer for electrodes that form cosmetic surfaces. Use 1500 grit for the core and cavity blocks. For a mirror finish, use 3000 grit, then finish with diamond compound and absorbent cotton. When fitting inserts, start with 400 grit and follow with 800 grit. Inserts in Japanese molds appear to be polished with 1000–1200 grit.
The main checks on a molded plastic gear are the tip-circle diameter and span measurement over several teeth. Gears that mesh too tightly or too loosely affect transmission performance. Use a dedicated gear measuring instrument for the span measurement.
Parts with uneven wall thickness can fill unevenly even when the gates are evenly spaced. Tian Jingdong’s mold 0004 is one example.
Gears molded from PC+30GF generally have better dimensional control and can usually be produced in a four-cavity mold. Their stiffness and wear resistance are lower than those of PBT+GF30 gears. PBT is harder to control dimensionally in this example and limits the mold to two cavities. A manufacturer such as Olympus still chose the higher-quality option despite the cost trade-off.
To keep the gate vestige from interfering with the part in use, recess the gate area so the trimmed vestige stays below the surrounding surface. Make the recess as shallow as possible while meeting that requirement. A typical depth is 0.3–0.5 mm. A deeper recess can affect molded dimensions, as in Tian Jingdong’s mold 0004 and Yi Xiangcheng’s mold 0026.
To improve filling at the end of the flow path, add vents and use additional inserts where needed. Plan these features before finalizing the mold layout. Aim for the most uniform melt pressure and temperature possible as the melt flows through the cavity.
Increasing the pinpoint gate size can improve fill in a thin-walled part that is difficult to mold, as in Wang Feng’s molds 0001 and 0002. An oversized gate can tear material out of the part during degating and leave a crater. It can also increase orientation and make the part more prone to warpage. A pinpoint gate diameter of Ø0.5–1.2 mm is suitable.
In electrical discharge machining (EDM), the spark gap is directly related to machining accuracy. The source gives a generally assumed ratio of 3:1 [2].
Typical taper angles for the retaining wedges on large core and cavity blocks are 1°, 3°, and 5°.
To facilitate ejection, make the lifter 0.1–0.3 mm shorter than nominal. This adds 0.1–0.3 mm to the local part wall thickness.
Consider the machining process for each mold component early in the design. Use milling and grinding where practical to minimize sinker EDM and wire EDM. The source favors milling and grinding for cost, accuracy, and machining time, while recognizing the accuracy of low-speed wire EDM.
Avoid designs that require sinker EDM over a large, simple flat surface. The operation takes time, makes accuracy difficult to maintain, and adds bench-fitting work.
Avoid stepped core and cavity blocks with large mating faces that must fit against each other. These features are often difficult to machine. The Mold Expert WeChat official account shares practical tooling advice.
With ultrasonic polishing, inconsistent feel and pressure control can distort the mold surface profile.
For a mold required to produce 10,000–15,000 parts per month, use NAK55 for the core and cavity blocks.
Mold Trials, Cavity Count, and Tool Construction
A capable injection molding machine can use five or more injection stages. For example, the first stage can fill the runner, the second can fill one-third of the part, and the third can fill one-half of the part. Examining the fill pattern at these points can help diagnose molding problems.
Consider using a multistage injection profile during mold trials for parts that are difficult to fill, have specified surface requirements, or have features that missed dimensional targets in earlier trials.
Japanese and Taiwanese injection molding machines can both use multistage injection. The source states that Taiwanese machines can also change injection pressure in addition to injection speed and another parameter that is missing from the source.
Determine the cavity count based on the molding cost per part, tooling cost allocated per part, part tolerances, and difficulty of manufacturing the mold.
When molding corrosive resins, select a corrosion-resistant tool steel or apply a protective surface treatment. When molding resins with glass fiber or other high-strength fillers, select mold components with suitable hardness.
Keep the cooling water passage more than 4 mm from the core or cavity block.
If the part is expected to be difficult to mold and require higher molding pressure, check the strength of the mold and reinforce the core and cavity blocks. Add support pillars and check the tolerances of the mating faces.
Avoid forced demolding in precision molds. It can affect production performance, dimensional accuracy, and the part surface.
Minimize slides and lifters where practical to reduce tooling cost and simplify manufacture.
If only 15–20 hundredths of a millimeter of stock remains on the blocks after milling, one roughing electrode and one finishing electrode are usually sufficient for a two- to four-cavity mold. This also applies to electrodes used to finish sharp corners.
When roughing a complex contoured surface by EDM, leave at least 0.06 in X and Y and at least 0.07 in Z for the finishing electrode.
Take extra care when using EDM electrodes with sharp corners, semicircular profiles, or hemispherical forms.
Determine the opening strokes of a three-plate pinpoint-gate mold as follows:
- Runner release between plates 101A and 102 = runner length + robot clearance (40–60 mm).
- Part removal between plates 102 and 103 = part size in the removal direction + robot clearance (70 mm).
Add tapped lifting holes to components that are hard to remove during assembly, such as retaining blocks, runner plates in three-plate molds, and core and cavity blocks. Where practical, two diagonally opposite fastening holes can be drilled and tapped through to accept lifting eyebolts.
When tight concentricity is required and the relevant features cannot be made on the same mold half, add a male and female tapered interlock between the halves if block size permits. This maintains concentricity during molding. Examples of roller molds with a #251 insert include 9018, 9026, 0004, and 0032.
For high-volume molds, consider the material of the mold base and slides. P20 is an option for both. Wear plates can also be fitted to the side slides.
Watch for machining distortion when grinding or milling mold components such as lifters that are less than 5 mm thick and more than 50 long, giving a length-to-thickness ratio above 10.
Cooling, Mold Fit, and Design Review

If the insert pocket is too deep for a cutter to reach the cooling ring groove, consider machining the groove in the underside of the block. Make the center boss slightly larger than the ring ID so the ring stays in the groove. If coolant flows on the inside, seat the ring ID against the mold wall. If coolant flows on the outside, seat the ring OD against the wall. Reversing this arrangement can cause leakage. The source specifically calls it oil leakage [3].
Minimize the difference between the coolant inlet and outlet temperatures. Keep it within 5°C for general molds and within 2°C for precision molds.
Cooling channel center-to-center spacing is typically 3–5 times the channel diameter. The distance from the channel wall to the cavity surface is typically 10–15 mm.
For higher-shrinkage resins such as polyethylene (PE), provide a cooling circuit in the direction of greatest part shrinkage.
When a mold has several cooling circuits, feed coolant first to the area closest to the sprue. The source asks how this instruction should be interpreted.
Use a relatively hard material such as SKH9 or STAVAX for the lifter. To improve production durability, fit an SKS3 wear plate under the lifter between the #106 ejector plate and the #107 ejector retainer plate. Use the same thickness as the ejector pin head. The Mold Expert WeChat official account shares practical tooling advice.
Forced demolding is generally possible when the undercut is below 3% [18]. Larger undercuts can scratch or even break the part during demolding. The allowable amount depends on the material. Softer materials such as PP and nylon can tolerate up to 5%, while PC and POM are limited to 2.5–3% in the source guidance.
Typical slide safety clearance is 1.5–5 mm.
Leave a small flat of roughly 0.8 mm at the root or crest of a molded plastic thread. This makes demolding easier and helps prevent damage to the thread surface.
A typical spacer block tolerance is +0.1 mm. For molds subject to high pressure, add support pillars. The specified pillar tolerance is typically +0.02–0.03 mm, and the pillar should stand 0.02–0.03 mm taller than the spacer block after assembly. The hardened surface of an S45C or S55C pillar is harder than the mold plate, which can settle during service and take up the extra height. If the pillar is 0.1 mm shorter than the spacer block, injection pressure can deflect plate #103. The resulting deflection at the core or cavity block can exceed 0.1 mm and cause flash.
The maximum heat-treatment distortion stated for PD613 (compared favorably with SKD11), PD555 (with SUS 420 J2), and NAK 101 (with SKD11) is 0.065/50. These steels are described as offering high wear and corrosion resistance and good mirror polishability for precision molds.
Vents are often machined along the parting surface and around the runner. For general molds, use a vent relief depth of about 0.5 mm and a vent land depth of 0.02 mm next to the part. For precision molds such as camera front and rear covers or housings, the relief depth is typically 0.07–0.1 mm and the land depth is 0.007–0.01 mm.
To ensure good contact between the mold halves, the parting surface generally stands 0.02 mm above the mold plate. C10–20 reliefs, 0.5–1 deep, are often milled at the four corners of plate #103 to prevent interference with plate #102.
The dimensional tolerance on a molded polyacetal part is around ±0.2%. The source estimates that each additional cavity increases the tolerance by about 5%, and gives a factor of 1.4 for an eight-cavity mold, yielding ±0.28% [4].
For NAK80, suitable cutting conditions given for a Kennametal Ø16 cutter with KCM25 inserts are a 0.4 mm depth of cut, a width of cut equal to two-thirds of the cutter diameter, a cutting speed of 55 m/min, a feed of 0.5 mm/rev, and air cooling.
A grinding machine can also produce a 0.5 mm groove.
The return pin has a hardened surface layer only about 0.5 mm deep, with a softer core.
For finish milling a flat surface, the stepover is typically two-thirds to four-fifths of the cutter diameter. Use a slow feed.
The slide slot tolerances are −0.01 and +0.01.
Review the part drawing with the customer before starting mold design. Confirm the parting line, ejector pin locations, undercut treatment, gate location and geometry, the relationship between wall thickness and shrinkage, and the tolerances. This helps clarify the customer’s design intent and improves the chances of getting the design right. Obtain agreement before making these decisions.
Hot Runners, Venting, and Precision Tooling
Hot runners are generally used for molds intended to produce 240,000 parts or more.
In tunnel-gated molds such as 9029 and 0031, the straight gate section often has a round or flat cross section. Eject it with a matching round or blade ejector pin. Because the pin is small and the gate section is long, insufficient draft can prevent clean ejection or break the pin. Provide 0.5°–1° of draft there.
The Olympus cg5375f1 rear cover used PC and a single-cavity mold with one pinpoint gate. Injection pressure reached 200 MPa on a Sumitomo 75-ton injection molding machine.
For a large runner system, lengthen the cold slug well accordingly. For example, the end of the sprue in mold 0039 was extended by 14 mm after the first mold trial.
Plan venting for large molds during design. A typical approach is to mill or grind a shallow groove around the mold perimeter, depending on the required accuracy. The groove should be shallower than the resin’s flash limit.
If an insert chamfer meets the surrounding core or cavity block, use a length tolerance of +0.05 from the insert bottom to the chamfer to prevent flash, as shown in the figure.
For standard EDM surfaces, a surface roughness of 7 µm is generally sufficient. Use 4 µm for general surfaces on precision molds and 2 µm where the cosmetic requirements are high. The source does not identify the roughness parameter.
Order mold steel stock 3–5 mm larger than the largest required finished dimension.
Avoid securing the sprue puller pin with a screw from the back. This can introduce stress and make the pin more likely to break. A mounting that allows some free movement is preferable.
Wire EDM typically leaves a 0.2 mm radius in an internal corner. Allow for this radius when designing insert pockets, square ejector pin holes, or other wire-cut features to avoid flash and burrs. The Mold Expert WeChat official account shares practical tooling advice.
Use a 2–3° taper per side where a slide mates with the core or cavity block. This helps reduce wear and makes it easier to preload the contact.
Coating thickness is typically 0.02–0.03 mm per side. Mold polishing stock is also typically 0.02–0.03 mm per side. Take both into account when coordinating part and mold dimensions.
Bench-fitting technique matters when fitting inserts. An insert should slide in slowly and smoothly. It should have no perceptible play when inserted one-quarter of the way into the pocket.
Mold rigidity is critical for dimensional accuracy when molding precision parts such as lenses and high-precision gears. Except for plates #102 and #103, other mold components made from S45C or S55C often require heat treatment to 45 HRC. The source attributes the exception to the core and cavity blocks normally standing proud of the mold plates [5].
For molded lenses, the source specifies YAG-250, a high-purity powder-metallurgy steel it attributes to Daido Steel, heat-treated to 56 ± 1 HRC [5].
Some molds have small round recesses that need polishing. When conventional methods are impractical, one option is an expensive fiber polishing stone. A simpler approach described in the source uses a toothpick held in a small radial drill at 6,000–10,000 rpm. Support the block by hand, apply diamond compound, and bring the area to be polished lightly into contact with the rotating toothpick.
The usual ejector pin recess depth is 0.1, with a tolerance of 0 to +0.02. For precision molding, use 0.03, with a tolerance of 0 to +0.01. In this case, strictly control the dimensions of the ejector retainer plate (upper ejector plate), ejector backing plate (lower ejector plate), ejector pin head counterbore depths, left and right support blocks, moving-side mold plate and block, ejector pin seating length, and overall ejector pin length.
Inspect molded parts in this order. Check the surface for burn marks and flow marks, the sidewalls for drag marks, and the part for complete fill. Check for flash at the parting line and along the shutoff witness lines, sink marks opposite thick sections, witness marks opposite the ejector pins, and the depth of the ejector pin recesses.
For a multi-cavity mold with stripper plate ejection, use one-piece core and cavity blocks on each half where possible. This helps keep ejection balanced.
Diamond compound in the #5000–#8000 grades can produce a mirror finish.
The stated radial runout for reaming is 0.05 mm.
The thread calculation for YKMA-0058 (Canon Oita front cover) is as follows. The nominal thread is M41 × 0.75. Pitch P = 0.75, major diameter D = 41, pitch diameter D2 = D − 0.649519 × P, minor diameter D1 = D − 1.082532 × P, and working thread height H1 = 0.541266 × P. The part shrinkage factor is S = 1.0058. The resulting mold block thread dimensions are pitch p1 = 0.75 × S, major diameter d1 = 41 × S, pitch diameter D2 = d1 − 0.649519 × p1, minor diameter D1 = d1 − 1.082532 × p1, and working thread height H1 = 0.541266 × p1.
An English-only section in the middle was deleted from the source.
Mold Opening, Cooling, and Inspection
Provide clearance around the ejector pin (EP) inside the core or cavity block to reduce friction, as shown in the figure.
For the small pull rod, a blue TL-type light-duty spring is typically selected to provide sufficient spring force.
An RLRT-type runner puller pin is typically used. Follow the dimensions shown in the figure. Make the clearance hole in plate 101 oversized by 0.2 across both sides, with no tolerance indicated. To ensure coaxial alignment, wire-cut the puller pin holes and the sprue bushing bore with plates 101 and 101A assembled. This prevents the pin from breaking when the two plates separate.
The arrangement shown below is commonly used to avoid inadequate venting.
Fiber-filled materials cause significant wear on the core and cavity blocks. Use separate inserts at wear-prone locations wherever practical.
If the support pillars cannot be laid out symmetrically on a large single-cavity mold, an asymmetric layout is acceptable provided there is no interference. It can also be used on molds with two or more cavities where appropriate.
The quality of a mold and the skill of its designer often show in the small details. Include microswitches and blocks that prevent unintended mold opening. The Mold Expert WeChat official account shares practical tooling advice.
QF-TE heat treatment consists of heating and hardening, followed by tempering.
Select the injection molding machine tonnage based on the molding area, clamping force, and mold size. A fourth force or pressure term is illegible in the source [6].
Two common pinpoint gate configurations are shown below. The relief depth B depends on the resin and angle A and is typically 0.5–0.6. Use a slightly deeper relief for ABS and PC.
A mold temperature of about 60°C is suitable for PPE. LCP has good moldability and can produce parts as thin as 0.14, as shown below.
Opening strokes for a three-plate mold:
PL1 = runner scrap length (vertical distance) + 10 for robot removal.
PL1 = distance from the sprue bushing inlet to the gate (relative distance) + 15 for automatic release.
PL2 = A + 2–3 mm.
For large parts or parts with cosmetic requirements, cooling channels are often built into the core and cavity blocks. Sometimes both the blocks and the plates are cooled. Cooling passages may also be drilled in slides and lifters. Lens molds use a grid-pattern cooling circuit. For some large housing, front-cover, rear-cover, and lens barrel molds, such as YKMA-1116, plates 101 and 101A also have hot-water passages. These maintain a stable temperature and help the mold open smoothly.
Pinpoint gate geometry and runner geometry are related.
Operator-induced measurement error is typically about 2 µm. When using a micrometer, take the reading after the ratchet clicks three times against the part. The specified measurement temperature is 22°C + 0.5°C [7].
Mirror-finish molds generally use insert ejection. On large parts, a single insert on #301 requires two pull rods. Uneven ejection can score the insert, especially when it has an irregular shape, as in molds 1024 and 1141. As shown below, relieve the bottom of the insert and fit a guide bushing in plate 104. Use screws and a round guide block to connect the insert and guide pin to plate 107. The assembly travels in the guide bushing for smoother operation during production.
PSF is less prone to static buildup but costs two to three times as much as PC. The source recommends PSF for premium products and PC for standard products.
For the parts in Figures 1 and 2, make the fixture shown in Figure 3 to measure the height of the raised features in Figure 2. Place the location indicated by the arrow in Figure 2 against the location indicated in Figure 3. Turn the fixture over to take the measurement.
Machine this mold in the following order:
- Leave the raised features unmachined and texture the flat surface first.
- Check the flatness and rework the mold until it meets the requirement.
- Machine all the raised features. The raised features on the molded part should be 0.03–0.05 mm lower than the two ribs on the side. Raise this point during the design review with the customer.
- Polish the raised features under 30–50× magnification. Even for routine polishing, 5× magnification is preferable. Mill the features on a machining center and leave about 0.03 mm for polishing. The source advises against EDM because it can leave the features uneven in size.
Mirror polishing can achieve a surface roughness of 0.05 µm. Leave 0.03 before polishing. For tighter accuracy, leave extra stock for later rework. Machine polishing gives a more uniform finish. The source does not specify the roughness parameter.
Gate Placement, Optical Parts, and Molding Setup
Put a tunnel gate on an angled face. This avoids direct melt impingement on the core or cavity block and helps prevent burn marks on the part. The Mold Expert WeChat official account shares practical tooling advice.
If burn marks appear at the gate, lower the injection pressure and injection speed to reduce melt shear.
Use color coding or surface elevation callouts when reviewing a part drawing. Keep the datum consistent. Use 0.00 for the datum, + for elevations above it, and − for elevations below it. The front and top views are generally sufficient. For complex parts such as housings, annotate all six views.
There are three types of coordinate measuring machine (CMM) probes:
Very thin, knife-edge sections of a part can become brittle under high molding pressure. Glass fiber reinforcement makes them even more prone to brittleness.
For the part shown below, use T = 2/3t. When the cosmetic surface has a fine texture, use T = 1/2t to reduce the risk of sink marks. The Mold Expert WeChat official account shares practical tooling advice.
For the illustrated part, gloss is less likely to appear on the cosmetic surface when T > 2/3t. A smaller angle A (30°) or the use of a radius R at the illustrated location further reduces the likelihood of gloss variation. The source attributes this to reduced melt backflow.
For the part shown below, lay out the pinpoint gates using the flow-length-to-wall-thickness ratio l/t. For high-flow resins, use l/t = 60–70, and up to 100 may be workable. Here l is the distance from the pinpoint gate to the farthest point, and t is the average wall thickness. Use l/t = 40–50 with 20% glass fiber or with irregular wall thickness.
The source groups the materials shown below into two categories. Crystalline resins, such as POM, PBT, and PP used for lens barrels, are described as having greater post-molding shrinkage and high water absorption. The source gives 48 h for dimensional measurements to stabilize. Amorphous resins include ABS and PC [8].
If dimensions in the 3D design have unilateral tolerances, ask the customer whether they can be changed to bilateral tolerances. To maintain the molded wall thickness across large, thin parts, add a gate. Some mold surfaces should be left slightly rougher. A mirror finish can create vacuum adhesion and make demolding difficult, even at #5000. A coarser finish can help. For optical lenses, the source specifies a steel nickel content above 15% [5].
The source lists three STAVAX grades: standard, MS, and ES for optical mirror finishes [5].
The source lists two SKD61 grades: standard and forged. The forged grade is described as having no directional properties and offering better performance.
ZDC2 casting alloy [9] is used for camera tripod screws and for the interchangeable-lens interface at the front of a camera.
For the illustrated part, use b = 1/4–1/3t and a = 1/2c. In Figure 2, place the one-sided groove in the gate flow direction to prevent the melt from directly impinging on the boss.
Allow enough clearance for robot part removal when designing the mold.
The source gives a fastest mold change time of 6 seconds for a fully automatic system and a cost of 200,000 for one injection molding machine, with no currency specified. Preheat the mold through the water passages. Design the passages to be preconnected, leaving only the supply and return ports to connect during the changeover. The source gives a mold change time of around 3 minutes in Taiwan.
In-mold degating is used frequently for optical parts.
Relationship between the runner system and part quality, particularly for molded lenses:
When checking mold strength, consider the machine clamping force and the strength of the mold plates and core and cavity blocks.
Inserts can be held by vacuum.
A cavity pressure sensor can be used to measure pressure loss inside the mold. For small parts, it is sometimes installed behind an ejector pin. For large parts, it may be mounted directly in the cavity.
Japanese injection molding machines can, according to the source, use up to 10 stages of settings for pressure and injection speed. On higher-quality machines, the settings generally remain stable once set.
The nozzle contact force is around 6 tons. On injection molding machines rated below 45 tons, it is around 3 tons.
Surface Treatments, Temperature Control, and Toolmaking
Hard chrome plating can increase the surface hardness of beryllium copper. The beryllium copper component is generally cast.
Blasting media include glass grit, aluminum oxide, ground walnut shell, and steel grit.
Glass bead grit sizes include #200, #150, and #400. The #400 material resembles milk powder.
Relationship between molding materials and mold production volume:
NAK-80 is used for low-volume molds. G = glass fiber. C = carbon fiber.
Hot runner systems are preferable for large business-machine components. The mold has a built-in heating system. The source lists three configurations: full hot runner, partial hot runner, and a further partial hot runner configuration [10].
See the figure below:
Thermal insulation plates are fitted at the front and rear of the mold where it mounts in the injection molding machine. They can be made from fiberglass laminate or phenolic board. The source puts the cost of fiberglass at five times that of phenolic board. It is used for high mold temperatures, optical parts, and molds running resins with more than 20% carbon fiber.
A slide can back off if the stop block is too small. Add a similar stop block or machine the leading end of the locking wedge to a sharper point.
The source lists water, chilled water (−5°C), oil, and electric heater rods under mold temperature control.
Wire EDM can cut a hole as small as 0.14 in diameter and 1 mm deep using Ø0.03 wire. Use a laser to make the wire start hole. The minimum hole diameter stated for chemical etching is Ø0.4.
Blade ejector pins are prone to flash and binding, so limit their use. A blade thickness of 0.5 or more is generally preferable. Below 0.5, the effective length is less than 10. The Mold Expert WeChat official account shares practical tooling advice.
The source lists two temperature sensor types, K (CA) and CI, and introduces their operating principles [11]:
If the insert is stationary, t can be as small as 0.2 mm. If the insert moves, use t = 0.5–0.7 mm (0.6 mm).
Common tool steels and their applicable hardness ranges:
Mold shrinkage rates for common plastics:
For raised lettering on the part, recess the lettering in the tool steel by direct engraving. For recessed lettering on the part, form the raised lettering on the tool steel by EDM. If the letters need to be glossier, as in the illustration, first EDM and polish the lettering to the required sheen. Then EDM the whole surrounding face, with relief in the electrode over the finished lettering. If the surrounding surface has a specified texture or cosmetic finish, apply the finish before machining the lettering.
Lens molds generally use a full-round runner, with one semicircle in the fixed half and one in the moving half. See the figure for the sprue puller pin profile.
For a two-plate mold with a sprue longer than 60, the design can omit a separate sprue bushing. Machine the fixed-side block to form the sprue bushing profile and taper the hole in plate 101 from the locating ring. During molding, the melt feeds directly into sprue inlet 201.
For the roller shown below, first grind the angled faces of the fixed-side and moving-side blocks, holding perpendicularity within 5 µm. Bolt the two blocks together and grind the flat faces until the joint line is difficult to see with the naked eye. Then wire-cut the hole.
Consider part orientation when designing a gear mold. For an external gear, position the wire EDM entry or seam on the block at the arrow shown in the figure [12].
A wire-cut insert can have rounded corners or square external corners. An internal wire-cut pocket will have corner radii. Match the radii on the mating features or square out the internal pocket corners for fitting, depending on the application.
For the callout PT1/4*15[%%C10], the source gives a threaded-hole diameter of 13.5 for 1/4 and 9.6 for 1/8 [13].
The cold slug well shown below grips the runner scrap. Machine it with a lathe tool.
Mold Maintenance, Inspection, and Coatings
Plastic or stamped parts often require printed markings. Test print adhesion by one of these methods:
- Wipe the marking with an ordinary organic solvent, gasoline, or alcohol.
- Apply a strong adhesive tape and pull it off quickly.
For complex molds with many inserts, perform maintenance after 10,000 shots, or about once a week. For simpler parts, the source gives 50,000 shots, or approximately every 10 days. Lubricate moving components during maintenance. Over an extended molding run, deposits from resin outgassing can accumulate on the mold and interfere with smooth operation.
Polish electrodes for coarse, intermediate, and fine cosmetic finishes using #800, #1200, and #1500–#2000 abrasive paper, respectively.
Use EDM dielectric oil or kerosene during polishing to keep residue from loading the paper or sticking to the workpiece. Clean with a degreasing solution after polishing.
Take measurements from at least three shots for a reliable dimensional check. For housing parts, the source describes a practice in Taiwan of checking five shots, with approximately three days of measurement work per shot.
If a drawing dimension cannot be inspected directly, discuss it with the customer and evaluate it at assembly.
Electroplating stack: ABS + Cu + Ni + Cr. The Cu layer is 20 µm, the Ni layer is 10 µm, and the Cr layer is 5 µm.
Vacuum deposition [14]: apply a 0.3–0.4 µm layer of pure gold.
Add a radius at the molded hook where possible and review it with the customer to reduce the risk of breakage.
As shown below, grinding can hold coaxiality and diameter, but the two indicated dimensions are harder to maintain.
Grinder designations: GC for internal and external cylindrical grinding, JG (GN) for cylindrical grinding, GF and GS for surface grinding, and GP for optical profile grinding [15].
The typical stock allowance before heat treatment is 0.20 mm. YORKEY has used as little as 0.04 mm and typically leaves 0.10 mm. An electric furnace sometimes replaces vacuum heat treatment, but can cause surface decarburization and blackening.
Optical Mold Machining and Measurement
Aspheric machining equipment costs cited in the source are NT$8 million for 0.1 µm, NT$12 million for 0.01 µm, and NT$20 million for 0.002 µm. Provide floor vibration isolation.
Mold plate and block requirements: parallelism of c to d is 0.005 for standard optics and 0.002 for special optics. For optical molds, hold perpendicularity and parallelism across all six faces below 0.002 mm. A 2 mm-deep relief in the center can help meet these requirements, as shown below.
The source gives 0.3 µm as the machining limit for the matte-finish test. For special optical components, use grinding where possible to maintain machining accuracy.
Standard lens barrel mold base sizes: 350 × 350 and 400 × 400.
When selecting an injection molding machine, check that the mold fits the machine and that the total shot weight is below the machine’s rated shot capacity.
The source groups optical parts into three categories: optical windows, standard optics, and special optics. The Japanese notation hon counts Newton interference fringes. More fringes indicate poorer part quality, and fewer indicate better quality. Five hon means five fringes. The actual value is the measured fringe count divided by 2, consistent with the source’s T/2 notation [16]. Use a reference master or a laser interferometer to inspect the part.
Reference masters are classified as follows. One primary master is used to check the reference masters. Reference masters are used to check the core or cavity blocks, and secondary masters are used during block machining.
For optical window lenses, place the parting surface 0.1–0.2 below the top surface, as shown below.
On the special optical lens shown below, cut the scribed line into the block with a diamond tool. A blurred line can result from incomplete filling or from machining a small flat where a sharp edge is required. See the arrows.
Optical window lens (PANEL): Use a single ejector rod located at the center of gravity.
When machining a spherical surface with SR0.1 mm, use a feed increment of 1 µm or 2 µm.
Set the core or cavity block tolerance to one-fifth of the part tolerance. Set the electrode tolerance to one-half of the block tolerance.
To measure small radii such as R0.14 and R0.002, use an electron microscope at 500× magnification. At 50,000×, the source calls for switching off an unidentified function and measuring automatically [17].
Use the vent dimensions shown below. Provide vents first at the locations indicated on the runner and part drawings.
For angular tolerances tighter than 30′, use a purpose-built machining fixture and a surface grinder.